Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 15.5 cSt | 15.5 cSt | Toluene Solution; Finaprene 1008 Test |
Total Finaprene® 503 Styrene-Butadiene TPE Copolymer
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 503 is a thermoplastic elastomer type linear butadiene-butadiene block copolymer (SBS). Thanks to its high styrene content, Finaprene® 503 provi.. |