Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 144 cSt | 144 cSt | Styrene solution viscosity 5%; ASTM D-1416 |
Dynasol Solprene® 200P Polybutadiene Rubber Solprene 200P is a medium cis polybutadiene partially branched to reduce cold flow and improve processability. Solprene 200P has excellent mixing and processing behavior, is used as ingredient for p.. |