Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.025 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.025 cm/cm

@Time 86400 sec
0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific)
LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.025 cm/cm

@Time 86400 sec
0.025 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific)
LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.025 cm/cm

@Time 86400 sec
0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer
LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.025 cm/cm

@Time 86400 sec
0.025 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer
LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.025 cm/cm

@Time 86400 sec
0.025 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.025 cm/cm

@Time 86400 sec
0.025 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA
LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermotuf V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.025 - 0.027 cm/cm

@Time 86400 sec
0.025 - 0.027 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific)
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Copyright © lookpolymers.com All Rights Reserved