Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0244 cm/cm @Time 86400 sec |
0.0244 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON RD000 PA 66 LNP STAT-KON* RD000 is a compound based on Nylon 66 resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |