Linear Mold Shrinkage, Transverse 0.0224 cm/cm

@Time 86400 sec
0.0224 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer
LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.