Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0135 cm/cm @Time 86400 sec |
0.0135 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON RFD04 PA 66 LNP STAT-KON* RFD04 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Electrically Conductive. |