Polymer Property : Linear Mold Shrinkage, Transverse = 0.0133 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0133 cm/cm

@Time 86400 sec
0.0133 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000 PP
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0133 cm/cm

@Time 86400 sec
0.0133 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific)
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0133 cm/cm

@Time 86400 sec
0.0133 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY M3000 PP
LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat.