Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0098 cm/cm @Time 86400 sec |
0.0098 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0098 cm/cm @Time 86400 sec |
0.0098 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.0098 cm/cm @Time 86400 sec |
0.0098 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0098 - 0.0099 cm/cm @Time 86400 sec |
0.0098 - 0.0099 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10 LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0098 cm/cm @Time 86400 sec |
0.0098 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Linear Mold Shrinkage, Transverse | 0.0098 cm/cm @Time 86400 sec |
0.0098 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized. |