Polymer Property : Linear Mold Shrinkage, Transverse = 0.0048 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0048 - 0.0054 cm/cm

@Thickness 2.00 mm
0.0048 - 0.0054 in/in

@Thickness 0.0787 in
ASTM D955
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Linear Mold Shrinkage, Transverse 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC
LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC
LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES
LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific)
LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UV00ASU PPA
LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural.
Linear Mold Shrinkage, Transverse 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UV00AS PPA
LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.