Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0046 cm/cm

@Time 86400 sec
0.0046 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea..
Linear Mold Shrinkage, Transverse 0.0046 cm/cm

@Time 86400 sec
0.0046 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific)
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System.
Linear Mold Shrinkage, Transverse 0.0046 cm/cm

@Time 86400 sec
0.0046 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA
LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized.