Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0042 - 0.0043 cm/cm @Thickness 2.00 mm |
0.0042 - 0.0043 in/in @Thickness 0.0787 in |
ASTM D955 |
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Linear Mold Shrinkage, Transverse | 0.0042 - 0.0046 cm/cm @Thickness 1.00 mm |
0.0042 - 0.0046 in/in @Thickness 0.0394 in |
ASTM D955 |
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |