Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0036 - 0.0040 cm/cm

@Time 86400 sec
0.0036 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0036 - 0.0040 cm/cm

@Time 86400 sec
0.0036 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0036 cm/cm

@Time 86400 sec
0.0036 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI
LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.