Polymer Property : a Lattice Constant = 5.139 Å Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
a Lattice Constant 5.139 Å
5.139 Å
Mateck YSZ
Substrate bicrystals for superconductivity