Polymer Property : a Lattice Constant = 5.125 Ã… Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
a Lattice Constant 5.125 Ã…
5.125 Ã…
Mateck Zirconium Oxide Substrate, ZrO2:Y(9.5% Y)
Substrate single crystals for superconductivity