Polymer Property : a Lattice Constant = 4.64 Ã… Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
a Lattice Constant 4.64 Ã…
4.64 Ã…
Mateck Magnesium Fluoride (MgF2)
Optical crystals