Physical Properties | Metric | English | Comments |
---|---|---|---|
a Lattice Constant | 4.216 Ã… | 4.216 Ã… | |
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 13%. |