Polymer Property : a Lattice Constant = 3.905 Ã… Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
a Lattice Constant 3.905 Ã…
3.905 Ã…
MarkeTech Strontium Titanate (SrTiO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
a Lattice Constant 3.905 Ã…
3.905 Ã…
Mateck Nb:SrTiO3
Substrate bicrystals for superconductivity
a Lattice Constant 3.905 Ã…
3.905 Ã…
Mateck SrTiO3
Substrate bicrystals for superconductivity