Polymer Property : a Lattice Constant = 3.685 Ã… Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
a Lattice Constant 3.685 Ã…
3.685 Ã…
Mateck NdCaAlO4
Substrate single crystals for superconductivity