Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | >= 9.17 hour | >= 9.17 hour | to 25 psi drop; ASTM D2272 |
ChevronTexaco Regal® 220 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |