Polymer Property : Oxidative Stability = 7000 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Stability >= 7000 hour
>= 7000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 32 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 7000 hour
>= 7000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 46 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 7000 hour
>= 7000 hour
Hours to 2 mg KOH/g acid number; ASTM D943
ChevronTexaco Regal® 46 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Oxidative Stability 7000 hour
7000 hour
ASTM D 943
ConocoPhillips Hydroclear® 100 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Oxidative Stability 7000 hour
7000 hour
ASTM D 943
ConocoPhillips Hydroclear® MV100 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Oxidative Stability 7000 hour
7000 hour
ASTM D 943
ConocoPhillips Hydroclear® MV32 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Oxidative Stability 7000 hour
7000 hour
ASTM D 943
ConocoPhillips Hydroclear® MV46 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Oxidative Stability 7000 hour
7000 hour
ASTM D 943
ConocoPhillips Hydroclear® MV68 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Oxidative Stability >= 7000 hour
>= 7000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 22 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 7000 hour
>= 7000 hour
Hours to 2 mg KOH/g acid number; ASTM D943
ChevronTexaco Regal® 32 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..