Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | >= 6500 hour | >= 6500 hour | Hours to 2 mg KOH/g acid number; ASTM D943 |
ChevronTexaco Regal® 68 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Oxidative Stability | 6500 hour | 6500 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil 797 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Oxidative Stability | 6500 hour | 6500 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil 797 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |