Polymer Property : Oxidative Stability = 5500 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Stability 5500 hour
5500 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil 798 Mobil DTE 790 Series
Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life..
Oxidative Stability 5500 hour
5500 hour
ConocoPhillips 100 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5500 hour
5500 hour
ConocoPhillips 32 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5500 hour
5500 hour
ConocoPhillips 46 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5500 hour
5500 hour
ASTM D 943
ConocoPhillips Hydroclear® 150 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Oxidative Stability 5500 hour
5500 hour
ConocoPhillips 68 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5500 hour
5500 hour
ConocoPhillips MV32 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5500 hour
5500 hour
ConocoPhillips 22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5500 hour
5500 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil 798 Mobil DTE 790 Series
Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life..