Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Stability 5000 hour
5000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Light Mobil DTE Oil Named Series
The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se..
Oxidative Stability >= 5000 hour
>= 5000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco 115 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability 5000 hour
5000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Light Mobil DTE Oil Named Series
The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se..
Oxidative Stability 5000 hour
5000 hour
ASTM D 943
ConocoPhillips Hydroclear® 150 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Oxidative Stability 5000 hour
5000 hour
ConocoPhillips 150 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Oxidative Stability 5000 hour
5000 hour
ASTM D 943
ConocoPhillips Hydroclear® 320 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..