Polymer Property : Oxidative Stability = 268 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Stability 268 hour
268 hour
Rotating Bomb Oxidation Test (RBOT); ASTM D2272
ExxonMobil Teresstic N Series 320
The Teresstic N Series products are premium-quality oils specifically designed to meet the demanding requirements of modern industrial paper machine circulating systems. They are engineered to provi..
Oxidative Stability 268 hour
268 hour
Rotating Bomb Oxidation Test (RBOT); ASTM D2272
ExxonMobil Teresstic N Series 320
The Teresstic N Series products are premium-quality oils specifically designed to meet the demanding requirements of modern industrial paper machine circulating systems. They are engineered to provi..