Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 26.67 hour | 26.67 hour | 25 psi pressure drop; ASTM D2272 |
ChevronTexaco GST® EP ISO 32 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |