Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 2500 hour | 2500 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Oxidative Stability | >= 2500 hour | >= 2500 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco ISO 220 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Oxidative Stability | >= 2500 hour | >= 2500 hour | Hours to 2 mg KOH/g acid number; ASTM D943 |
ChevronTexaco Regal® 220 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil Teresstic 32 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 220 Gear Oil AGMA Lubricant No. 5 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 320 Gear Oil AGMA Lubricant No. 6 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 460M Gear Oil AGMA Lubricant No.7EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 100M Gear Oil AGMA Lubricant No. 3EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 460 Gear Oil AGMA Lubricant No. 7 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 68 Gear Oil AGMA Lubricant No. 2 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 680 Gear Oil AGMA Lubricant No. 8EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 150 Gear Oil AGMA Lubricant No. 4 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 100 Gear Oil AGMA Lubricant No. 3 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Oxidative Stability | 2500 hour | 2500 hour | Oxidation Control; ASTM D-2893 |
ConocoPhillips 220M Gear Oil AGMA Lubricant No. 5EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |