Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 23.33 hour | 23.33 hour | 25 psi pressure drop; ASTM D2272 |
ChevronTexaco GST® ISO 100 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Oxidative Stability | 23.33 hour | 23.33 hour | 25 psi pressure drop; ASTM D2272 |
ChevronTexaco GST® ISO 68 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Oxidative Stability | 23.33 hour | 23.33 hour | 25 psi pressure drop; ASTM D2272 |
ChevronTexaco GST® ISO 46 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |