Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 1800 hour | 1800 hour | |
ChevronTexaco ISO 220 Paper Machine Oil D FeaturesChevron Paper Machine Oils D are manufactured using select high viscosity index, paraffinic base stocks. Their additive packages include rust, oxidation, and foam inhibitors as well as an ef.. |