Polymer Property : Oxidative Stability = 18.53 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Stability 18.53 hour
18.53 hour
25 psi pressure drop; ASTM D2272
ChevronTexaco ISO 32 Turbine Oil TR
FeaturesChevron Turbine Oil TR is a premium quality turbine oil designed to meet the critical demands of bearings subjected to high temperatures.It is formulated with ISOSYN™ base stocksThis ISO 32..