Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 17000 hour | 17000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco GST® ISO 32 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |