Physical Properties Metric English Comments
Oxidative Stability >= 16.7 hour
>= 16.7 hour
25 psi pressure drop; ASTM D2272
ChevronTexaco ISO 32 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 16.7 hour
>= 16.7 hour
to 25 psi drop; ASTM D2272
ChevronTexaco Regal® 46 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Oxidative Stability >= 16.7 hour
>= 16.7 hour
25 psi pressure drop; ASTM D2272
ChevronTexaco ISO 22 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 16.7 hour
>= 16.7 hour
to 25 psi drop; ASTM D2272
ChevronTexaco Regal® 32 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Copyright © lookpolymers.com All Rights Reserved