Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | >= 14000 hour | >= 14000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco ISO 32 Turbine Oil TR FeaturesChevron Turbine Oil TR is a premium quality turbine oil designed to meet the critical demands of bearings subjected to high temperatures.It is formulated with ISOSYN™ base stocksThis ISO 32.. |