Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 14.17 hour | 14.17 hour | RPVOT; ASTM D2272 |
ConocoPhillips Syncon® 220 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Oxidative Stability | 14.17 hour | 14.17 hour | RPVOT; ASTM D2272 |
ConocoPhillips Syncon® 460 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |