Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | 1250 hour | 1250 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Oxidative Stability | 1250 hour | 1250 hour | Turbine Oil Stability Test (TOST); ASTM D943 |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |