Physical Properties Metric English Comments
Oxidative Stability >= 1000 hour
>= 1000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Teresstic 220
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Oxidative Stability >= 1000 hour
>= 1000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Teresstic 320
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Oxidative Stability >= 1000 hour
>= 1000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Teresstic 460
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Oxidative Stability >= 1000 hour
>= 1000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 220 Machine Oil AW
FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu..
Oxidative Stability >= 1000 hour
>= 1000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 320 Machine Oil AW
FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu..
Oxidative Stability 1000 hour
1000 hour
ChevronTexaco ISO 320 Paper Machine Oil D
FeaturesChevron Paper Machine Oils D are manufactured using select high viscosity index, paraffinic base stocks. Their additive packages include rust, oxidation, and foam inhibitors as well as an ef..
Oxidative Stability >= 1000 hour
>= 1000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 460 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 1000 hour
>= 1000 hour
Hours to 2.0 mg KOH/g acid number; ASTM D943
ChevronTexaco ISO 680 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
Oxidative Stability >= 1000 hour
>= 1000 hour
Hours to 2 mg KOH/g acid number; ASTM D943
ChevronTexaco Rando® HD 220
Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow..
Oxidative Stability >= 1000 hour
>= 1000 hour
Hours to 2 mg KOH/g acid number; ASTM D943
ChevronTexaco Regal® 460 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Oxidative Stability >= 1000 hour
>= 1000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Teresstic 220
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Oxidative Stability >= 1000 hour
>= 1000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Teresstic 320
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Oxidative Stability >= 1000 hour
>= 1000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ExxonMobil Teresstic 460
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Copyright © lookpolymers.com All Rights Reserved