Polymer Property : Coating Weight = 70.0 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 70.0 - 85.0 g/m²
43.8 - 53.1 lb/ream
per side
ArcelorMittal Extragal® Z140 Double-sided pure zinc galvanized steel
Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib..
Coating Weight 70.0 - 85.0 g/m²
43.8 - 53.1 lb/ream
per side
ArcelorMittal Ultragal® Z140 Zinc coatings and thin organic coating
Applications: With its ability to limit repeated waviness during deformation, combined with the proven qualities of Extragal(surface quality, corrosion protection), Ultragal is a coating specificall..