Coating Weight >= 7.00 g/m²
>= 4.38 lb/ream
BTM 14922
Borealis CA7230 Low Density Polyethylene
CA7230 is a low-density polyethylene for extrusion coating. CA7230 contains no additives. Applications: Extrusion coating of high volume production of boards and papers. Coating of various plasti..