Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 6.00 g/m² | 3.75 lb/ream | BTM 00117 |
Borealis Borstar® CB9600 HDPE for Extrusion Coating Borstar CB9600 is the first bimodal high-density coating grade produced using the unique Borstar PE technology. The process controls the polymer `s molecular structure and is designed to produce bi.. |