Physical Properties Metric English Comments
Coating Weight >= 90.0 g/m²
>= 56.3 lb/ream
double-sided
ArcelorMittal Zagnelis™ ZM90 Double-sided ZnMgAl galvanized steel
Presentation: Zagnelis™ coating has been specially designed to improve corrosion protection of vehicles, while satisfying OEMs' specifications regarding manufacturability: stamping, welding, adhesi..