Polymer Property : Coating Weight = 5.00 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight >= 8.00 g/m²
>= 5.00 lb/ream
TAPPI test method; ASTM D539
NOVA Chemicals Novapol® LC-0522-A LDPE Extrusion Resin
Excellent sealability, High drawdown, High adhesion, Good barrier, High stiffness, Good abrasion resistanceApplications: Milk cartons, Paperboard containers, Liquid packaging, Woven fabrics, Lumber ..
Coating Weight >= 8.00 g/m²
>= 5.00 lb/ream
BTM 14922
Borealis CG8410 High Density Polyethylene
CG8410 is a high-density polyethylene for extrusion coating. Applications: extrusion coating of high volume production of boards and papers.Information provided by Borealis AG
Coating Weight >= 8.00 g/m²
>= 5.00 lb/ream
Extrusion Coating Processability; Dow Method
Dow 4010 Low Density Polyethylene (LDPE)
Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc..