Polymer Property : Coating Weight = 5.00 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight >= 5.00 g/m²
>= 3.13 lb/ream
BTM 14922
Borealis CA9150 Low Density Polyethylene
CA9150 is a low-density polyethylene for extrusion coating. CA9150 contains no additives. Applications: coating and lamination of aluminum foil, coating of various plastic films and cellophane, and..