Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 42.2 g/m² | >= 26.4 lb/ream | 520 |
ExxonMobil Label-Lyte® 85 LP-200M Mirror Finish, Metallized, White Opaque OPP for Water-based Patch Label Applications White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. It has an anti-static, "mirror finish" metallized print surface that is coro.. |