Polymer Property : Coating Weight = 36.6 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 36.6 g/m²
22.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 40MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle Ea..
Coating Weight 36.6 g/m²
22.9 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 40LL666 OPP Film
Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..