Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 50.9 g/m² | 31.8 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 57LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |