Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 29.9 g/m² | 18.7 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 32MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin.. |