Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 44.8 g/m² | 28.0 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 50LL210 OPP Film Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Coating Weight | 44.8 g/m² | 28.0 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ ROSO 50LR210 OPP Film Product Description: A clear, machine-direction shrinkable, one-side treated, polypropylene film. This film is designed for use as a monoweb in roll-fed labeling of contoured containers, such as alu.. |
|||
Coating Weight | 44.8 g/m² | 28.0 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 50TD200 Preliminary Data Sheet OPP Film Product Description: A clear, transverse-direction shrinkable, one-side treated, polyolefin film. With a density below 1.0, this film facilitates floatation and supports the PET bottle-to-bottle rec.. |