Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Coating Weight = 27.3 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight >= 43.7 g/m²
>= 27.3 lb/ream
520
ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications
Coated, white, metallized polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. This film is compatible with offset litho and UV-cured in..