Polymer Property : Coating Weight = 25.1 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 25.1 g/m²
15.7 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 110 AXT OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur..
Coating Weight 25.1 g/m²
15.7 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 40MW648 OPP Film
Product Description: A high speed super white opaque, biaxially oriented polypropylene film coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provides an excel..
Coating Weight 25.1 g/m²
15.7 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 40MW647 OPP Film
Product Description: A super white opaque, biaxially oriented polypropylene film acrylic coated two sides. Provides outstanding performance on all types of packaging machines.Availability: Africa & ..