Polymer Property : Coating Weight = 22.2 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 22.2 g/m²
13.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 100 AB-X OPP Film
Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as..
Coating Weight 22.2 g/m²
13.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 25MB666 OPP Film
Product Description: A Biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Coating Weight 22.2 g/m²
13.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 25MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low seal temperature (VLTS) coating. VLTS coating provides excellent perf..
Coating Weight 22.2 g/m²
13.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 25MBT666 OPP Film
Product Description: Biaxially oriented polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping offering unique aspect and cost reduction advant..
Coating Weight 22.2 g/m²
13.9 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 310 AB OPP Film
Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in applications, including overwrap, horizontal, and vertical packaging. This film is suitable ..