Polymer Property : Coating Weight = 21.8 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 21.8 g/m²
13.6 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 25ICT OPP Film
Product Description: A one-side sealable, very broad seal range coextruded BOPP. This film is designed for use in unsupported plain or surface printed high-speed horizontal applications. The enhance..